Ibigize imiti

Ibigize imiti

Cr

Ni

Mo

Co

Cb + Ta

Al

Ti

C

Fe

Me

Mn

Si

P

S

Indangagaciro (ntarengwa)

20.0

 

8.0

-

3.15

-

-

-

-

 

-

-

-

-

% Indangagaciro (ntarengwa)

23.0

bal

10.0

1.0

4.15

0.4

0.4

0.1

5.0

 

0.5

0.5

0.015

0.015

Ibikoresho bya mashini

Imashini & Ibintu bifatika

21 ° C.

204 ° C.

316 ° C.

427 ° C.

538 ° C.

649 ° C.

760 ° C.

871 ° C.

Imbaraga Zihebuje / Mpa

992.9

923.9

910.1

910.1

896.3

820.5

527.8

275.8

0.2% Gutanga Imbaraga / MPa

579.2

455.1

434.4

420.6

420.6

413.7

406.8

268.9

Kurambura%

44

45

42.5

45

48

34

59

117

Coefficient yo Kwagura Ubushyuhe
um / moC

-

13.1

13.3

13.7

14

14.8

15.3

15.8

Imyitwarire yubushyuhe /kcal/(hr.mc)

8.5

10.7

12.2

13.5

15

16.4

17.9

19.6

Modulus ya Elastique / MPa

2.07

1.93

1.93

1.86

1.79

1.65

1.59

-

Porogaramu

625 URUPAPURO RWA DATA

Moteri ya moteri ya moteri

Sisitemu yo gusunika moteri

Sisitemu yo gutwara indege

Turbine impeta y'impuzu

Guhuza no kwagura ingingo

Components Ibigize amazi yo mu nyanja

Equipment Ibikoresho byo gutunganya imiti

Kurwanya ruswa

Alloy 625 yihanganiye ibidukikije byinshi byangirika. Muri alkaline, amazi yumunyu, amazi meza, umunyu utabogamye, no mwikirere, hafi nta gitero kibaho. Nikel na chromium bitanga imbaraga zo kurwanya ibidukikije. Nickel na molybdenum bitanga imbaraga zo kutagira umwuka wa okiside.

Gutobora no gutobora birindwa na molybdenum. Niobium ituma amavuta arwanya ubukangurambaga mugihe cyo gusudira. Chloride guhangayika-kwangirika kumeneka ni byiza. Amavuta arwanya gupima no okiside ku bushyuhe bwinshi.

4Cr14Ni14W2Mo kare

Ibarura

URUBUGA RWA PRODUCT

URUPAPURO RWA SIZE

SIZE RANGE TO

Amavuta 625

0.5 muri

8 muri

Amavuta 625

0,25 mm

3.18 mm

Amashanyarazi 625 yo gusudira

0,5 mm

3.175 mm

Kuvanga urupapuro 625

0,25 mm

76.2 mm

Kuvanga umurongo 625

Mm 12

260 mm

Amavuta 625

0.5 muri

8 muri

Amavuta 625

0.5 muri

8 muri

Umuco w'isosiyete

Indangagaciro Nkuru: Nziza, Guhanga udushya, Kuba inyangamugayo no gutsinda-gutsinda

Ihame rya serivisi: Shiraho agaciro kubakiriya, Guhaza abakiriya


  • Mbere:
  • Ibikurikira:

  • Andika ubutumwa bwawe hano hanyuma utwohereze