Austenite Ibyuma

Ibicuruzwa birambuye

Ibicuruzwa

Ubushyuhe bwo hejuru

◆ 904L ntishobora gukemura gusa ruswa rusange ya acide sulfurike, aside fosifori na acide acike, ariko kandi ikemura ibibazo bya chloride itera ruswa, ruswa ya ruswa hamwe na ruswa.

◆ 253Ma (S30815) nicyuma cyihanganira ubushyuhe cyuma cya austenitike kitagira ibyuma cyakozwe hashingiwe kuri 21Cr-11Ni ibyuma bitagira umuyonga binyuze muri N alloying no kongeramo ibintu bidasanzwe Ce. Ikoreshwa cyane cyane mugukora amasahani.

◆ 254SMo (F44 / S31254) nicyuma cyo hejuru cyane cya austenitis cyuma kitagira umuyonga, gikunze gukoreshwa mugusimbuza nikel nyinshi na titanium. Ikoreshwa cyane mubikorwa byinshi byangirika nka chimique na peteroli na choride ibisubizo.

◆ Al-6XN (N08367) ikwiranye na pompe, valve, flanges hamwe na sisitemu yo kuvoma peteroli na gaze, imiti n’amashanyarazi.

Ibigize imiti

Icyiciro

C

Si

Mn

S

P

Cr

Ni

Mo

Cu

N

ikindi

ntarenze

904L

0.02

1

2

0.015

0.03

19 ~ 21

24 ~ 26

4 ~ 5

1 ~ 2

-

-

253Ma

0.05 ~ 0.1

1.4 ~ 2

0.8

0.03

0.04

20 ~ 22

10 ~ 12

-

-

0.14 ~ 0.2

Ce0.03 ~ 0.08

254So

0.02

0.8

1

0.01

0.03

19.5 ~ 20.5

17.5 ~ 18.5

6 ~ 6.5

0.5 ~ 1

0.18 ~ 0.22

-

Al-6XN

0.03

1

2

0.03

0.04

20 ~ 22

23.5 ~ 25.5

6 ~ 7

≤0.75

0.18 ~ 0.25

-

Kugabanya umutungo ntarengwa

Icyiciro

leta

imbaraga zingana RmN / m㎡

Imbaraga Zitanga Rp0.2N / m㎡

Kurambura Nka%

Brinell gukomera HB

904L

Umuti

490

215

35

-

253Ma

Umuti

650

310

40

210

254So

Umuti

650

300

35

-

Al-6XN

Umuti

835

480

42

-