Incoloy
Ubushyuhe bwo hejuru
◆ Incoloy800H (Ns112 / N08810), Incoloy800HT, Incoloy800 (Ns111 / N08800) ni ibicuruzwa bitatu bigize urukurikirane rumwe rwa nikel-fer-chromium alloy, birwanya ruswa, birwanya ruswa hamwe nubushyuhe bwo hejuru bwa okiside, bikoreshwa mubushuhe kuvura Ibikoresho byo kwishyiriraho, bitwikiriye ibikoresho byo kurwanya alloy tubular ubushyuhe, ibikoresho byo gutunganya imiti na peteroli.
◆ Incoloy825 (Ns142 / N08825) ni umusemburo rusange wubwubatsi. Ifite anti-acide na alkali ibyuma byangirika muri okiside no kugabanya ibidukikije. Ibintu byinshi bya nikel bituma amavuta agira imbaraga zo kurwanya ruswa. Ikoreshwa cyane mubice bitandukanye byinganda aho ubushyuhe bwo gukora butarenga 550 ° C.
◆ Incoloy901 ni imvura igwa, ibyuma birinda ubushyuhe. Amavuta afite imbaraga nyinshi zo gutanga umusaruro nimbaraga ziramba munsi ya 650 ° C, kurwanya okiside nziza munsi ya 760 ° C, kandi birahamye kubikoresha igihe kirekire. Ikoreshwa cyane mugukora ibice nkibice bihindagurika byindege na moteri ya gaz turbine moteri ikora munsi ya 650 ° C.
◆ Incoloy925 (N09925) nicyuma kivanze gifite imbaraga zumukanishi kandi zirwanya ruswa. Bikunze gukoreshwa mugukora ibice kubucukuzi bwa peteroli na gaze #ibikoresho.
◆ Incoloy926 nicyuma cya austenitike kitagira umuyonga gifite imiti isa na alloy 904L, ibirimo azote byiyongereye kugera kuri 0.2%, naho molybdenum ikaba 6.5%. Ahanini ikoreshwa mubwubatsi bwa marine, ibidukikije bya gaze ya acide, sisitemu ya gaz ya sulfure.
◆ Incoloy20 ni ubwoko bwibyuma bishobora gukora igihe kirekire munsi yubushyuhe buri munsi ya 600 ℃ hamwe na stress zimwe.
◆ Incoloy330 ifite imbaraga nyinshi, irwanya okiside nziza, irwanya ruswa, irwanya umunaniro mwiza, gukomera kuvunika nibindi bintu, kandi irakwiriye ingufu za kirimbuzi, inganda z’imiti, nizindi mashini.
Ibigize imiti
Icyiciro | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | ikindi |
ntarenze | |||||||||||||
Incoloy800 | 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 ~ 23 | 30 ~ 35 | shingiro | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | - |
Incoloy800H | 0.05 ~ 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 ~ 23 | 30 ~ 35 | shingiro | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | - |
Incoloy800HT | 0.06 ~ 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 ~ 23 | 30 ~ 35 | shingiro | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | Al + Ti 0,85 ~ 1.2 |
Incoloy825 | 0.05 | 0.5 | 1 | 0.03 | 0.03 | 19.5 ~ 23.5 | 38 ~ 46 | shingiro | ≤0.2 | 0.6 ~ 1.2 | 1.5 ~ 3 | 2.5 ~ 3.5 | - |
Incoloy901 | 0.1 | 0.6 | 1 | 0.03 | 0.3 | 11 ~ 14 | 40 ~ 45 | shingiro | ≤0.35 | 2.35 ~ 3.1 | ≤0.5 | 5 ~ 7 | Co≤1.0 |
Incoloy925 | 0.03 | 0.5 | 1 | 0.03 | 0.03 | 19.5 ~ 23.5 | 42 ~ 46 | shingiro | 0.15 ~ 0.5 | 1.9 ~ 2.4 | 1.5 ~ 3 | 2.5 ~ 3.5 | - |
Incoloy926 | 0.02 | 0.5 | 2 | 0.01 | 0.03 | 19 ~ 21 | 24 ~ 26 | shingiro | - | - | 0.5 ~ 1.5 | 6 ~ 7 | N15 ~ 0.25 |
Incoloy020 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5 ~ 26.5 | - | 13 ~ 16 | .5 1.5 | 0.3 ~ 0.7 | ≤0.5 | 2.5 ~ 3.7 | - |
Incoloy330 | 0.04 ~ 0.08 | 1 ~ 1.5 | 2 | 0.03 | 0.03 | 18 ~ 20 | 34 ~ 37 | shingiro | - | - | ≤1 | - | - |
Kugabanya umutungo ntarengwa
Icyiciro | leta | imbaraga zingana RmN / m㎡ | Imbaraga Zitanga Rp0.2N / m㎡ | Kurambura Nka% | Brinell gukomera HB |
Incoloy800 | Umuti | 500 | 210 | 35 | - |
Incoloy800H | Umuti | 450 | 180 | 35 | - |
Incoloy800HT | Umuti | 500 | 210 | 35 | - |
Incoloy825 | Umuti | 500 | 220 | 30 | - |
Incoloy901 | Umuti | 900 | 550 | 25 | - |
Incoloy925 | Umuti | 650 | 300 | 30 | - |
Incoloy926 | Umuti | 650 | 295 | 35 | - |
Incoloy20 | Umuti | 700 | 300 | 32 | - |
Incoloy330 | Umuti | 750 | 310 | 35 | - |