Monel

Ibicuruzwa birambuye

Ibicuruzwa

Ubushyuhe bwo hejuru

El Monel400 ifite imbaraga zo kurwanya ruswa muri acide hydrofluoric na gaze ya fluor, kandi ikwiranye na fitingi hamwe na valve zikoreshwa mu nganda zikora imiti, peteroli, ingufu za atome, no guteza imbere inyanja.

El Monel500 ifite imiterere myiza yubukanishi, imbaraga nyinshi hamwe no kurwanya ruswa. Irakwiriye kwizirika hamwe nibice byubatswe bikoreshwa munganda zikora imiti, amato nubwubatsi bwa marine.

El Monel404 ikoreshwa cyane mubikorwa bya peteroli, inganda za kirimbuzi, nibindi bikoresho bigezweho.

Ibigize imiti

Icyiciro

C

Si

Mn

S

P

Cr

Ni

Mo

Fe

Co

W

Al

Ti

Cu

ntarenze

Monel400

0.3

0.5

2

0.024

-

-

shingiro

-

≤2.5

-

-

-

-

28 ~ 34

Monel500

0.18

0.5

1.5

0.01

-

-

≥63

-

≤2

-

-

2.3 ~ 3.15

0.35 ~ 0.85

27 ~ 33

Monel404

0.15

0.1

0.1

0.024

-

-

52 ~ 57

-

≤0.5

-

-

≤0.05

-

Guma

Kugabanya umutungo ntarengwa

Icyiciro

Imiterere ya tekiniki

imbaraga zingana RmN / m㎡

Imbaraga Zitanga Rp0.2N / m㎡

Kurambura Nka%

Brinell gukomera HB

Monel400

Impimbano / ishyushye

516

170

35

-

Leta yegeranye

483

170

35

-

Monel500

Leta mpimbano + gusaza

960

686

20

27

igisubizo gikomeye + gusaza

896

585

20

24

Monel404

Leta yegeranye

550

185

36

-


  • Mbere:
  • Ibikurikira:

  • Andika ubutumwa bwawe hano hanyuma utwohereze