At Hangnie Super Alloys Co, Ltd., twumva uruhare rukomeye ibikoresho bikora neza bigira uruhare mubikorwa bitandukanye. Uyu munsi, tuzacengera mumitungo idasanzwe nibikorwa byo gukoraHastelloy C-276, nikel-alloy izenguruka umurongo uzwiho kurwanya bidasanzwe kwangirika.
Kurwanya ruswa ntagereranywa:
Hastelloy C-276 yihagararaho kubera kutagereranywa kwayo kwinshi kwangiza ibidukikije. Hano reba neza imbaraga zingenzi:
Itezimbere mu Kugabanya Ibidukikije: Iyi mavuta iruta ibidukikije bikuraho ogisijeni, bigatuma biba byiza muburyo butandukanye bwo gutunganya imiti.
Intsinzi ikomeye ya Oxidizing yumunyu: Hastelloy C-276 ikemura ibisubizo bikaze birimo chloride ferric na cupric byoroshye.
Nickel & Molybdenum Powerhouse: Ibirimo byinshi muribi bintu birinda amavuta kwirinda ruswa mu kugabanya ibidukikije.
Ibyiza bya Carbone Bike: Kugabanuka kwa karubone birinda imvura igwa ku mbibi za karbide mugihe cyo gusudira, bigatuma irwanya ruswa muri zone yasudutse.
Umwanya wo kwangirika kwangiritse: Ibi bikoresho birwanya neza ibitero byaho nko gutobora no gucika intege.
Nyampinga Kurwanya Ibibazo bya Chlorine: Imwe mumavuta make ashobora kwihanganira ingaruka mbi za gaze ya chlorine itose, hypochlorite, na dioxyde ya chlorine.
Hastelloy C-276: Ibintu bifatika iyo urebye
Ingingo yo gushonga: 1325-1370 ° C (Ingingo yo gushonga cyane isobanura kurwanya bidasanzwe ubushyuhe bwo hejuru)
Ubucucike: 8,90 g / cm3 (Ubucucike bwinshi bugira uruhare mu mbaraga no kuramba)
Inzira zibyara umusaruro (Icyitonderwa: Ibisobanuro byihariye birashobora gutandukana bitewe nuwabikoze)
Mugihe uburyo nyabwo bwo kubyaza umusaruro bushobora gutandukana gato hagati yababikora, dore urutonde rusange rwuburyo Hastelloy C-276 utubari tuzengurutswe:
Gushonga: Ibikoresho fatizo, birimo nikel, molybdenum, chromium, tungsten, hamwe nicyuma muburyo bukwiye, bishonga mumatanura ya vacuum induction (VIM) cyangwa guhuza VIM hamwe na electroslag remelting (ESR) kugirango isukure kandi ikureho umwanda.
Gutera: Icyuma gishongeshejwe noneho gisukwa mubibumbano kugirango bikore ingero zingana nubunini.
Gukora Bishyushye: Ingoti zikoreshwa mubikorwa bishyushye nko guhimba cyangwa gusohora kugirango ugere kumiterere isabwa no kunoza imiterere y'ibinyampeke hamwe nubukanishi.
Kuvura Ubushyuhe: Uburyo bwo gutunganya ubushyuhe bugenzurwa bishyirwa mubikorwa kugirango tunonosore imiterere yingano kandi tunoze neza ibikoresho byangirika kwangirika nimbaraga za mashini.
Kurangiza Ubuso: Intambwe yanyuma ikubiyemo inzira yo kurangiza hejuru nko gutunganya, gusya, cyangwa gusya kugirango ugere kumurongo wifuzwa kurangiza no kwihanganira ibipimo.
Kugenzura ubuziranenge: Igenzura rikomeye ryigenzura rikorwa mubikorwa byose kugirango harebwe niba utubari twujuje ibyangombwa byose bigize imiti, imiterere yubukanishi, nibisabwa murwego.
Hangnie Super Alloys: Umufatanyabikorwa Wizewe kuri Hastelloy C-276
Muri Hangnie Super Alloys Co., Ltd., twiyemeje guha abakiriya bacu ubuziranenge bwiza bwa Hastelloy C-276. Ubuhanga bwacu muguhitamo ibikoresho, gutunganya umusaruro, no kugenzura ubuziranenge byemeza ko wakiriye ibicuruzwa bitanga imikorere idasanzwe no kuramba ndetse no mubidukikije bisabwa cyane.
Kubaza cyangwa kumenya byinshi byukuntu Hastelloy C-276 ishobora kugirira akamaro ibyifuzo byawe, wumve nezatwandikireUyu munsi.