Nickel

  • Nickel

    Ubushyuhe Bwinshi Bwuzuye Imiti Yumuti Grade Ni Fe Cu C Mn S Si Nickel200 99 ≤0.4 ≤0.25 ≤0.15 ≤0.35 ≤0.01 ≤0.35 Nickel201 99 ≤0.4 ≤0.25 ≤0.02 ≤0.35 .