Nitronic

  • Nitronic

    Ubushyuhe Bwinshi Buvanze Imiti Yumuti Icyiciro C Si Mn SP Cr Ni Fe Mo Ti Cu Nb N ibindi bitarenze Nitronic50 0.06 1 4 ~ 6 0.03 0.04 20.5 ~ 23.5 11.5 ~ 13.5 shingiro 1.5 ~ 3 - - 0.1 ~ 0.3 0.2 ~ 0.4 - Nitronic60 0.1 3.5 ~ 4.5 7 ~ 9 0.03 0.04 16 ~ 18 8 ~ 9 shingiro - - - - 0.08 ~ 0.18 - Alloy imitungo ntarengwa Icyiciro cya leta imbaraga zingana RmN / m㎡ Imbaraga Zitanga Rp0.2N / m㎡ Kurambura Nka% B ...