Ibigize imiti
Amavuta | element | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Amavuta B2 | Min | 26.0 | |||||||||
Icyiza | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Kuringaniza | 1.0 | 30.0 | 2.0 | 1.0 |
Ibikoresho bya mashini
Imiterere ya Aolly | Imbaraga Rm Mpa Min | Tanga imbaraga RP 0. 2 Mpa Min | Kurambura A 5% Min |
Igisubizo | 745 | 325 | 40 |
Ibintu bifatika
Ubucucike g / cm3 | Ingingo yo gushonga ℃ |
9.2 | 1330 ~ 1380 |
Bisanzwe
Inkoni, Akabari, Umugozi no guhimba ububiko- ASTM B 335 (Inkoni, Akabari), ASTM B 564 (Guhimba), ASTM B 366 (Bikwiye)
Isahani, urupapuro na Strip- ASTM B 333
Umuyoboro na Tube- ASTM B 622 (Ikidodo) ASTM B 619 / B626 (Umuyoboro Weld)
Ibiranga Hastelloy B2
Resistance Kurwanya bikomeye guhangayikishwa no kwangirika
Resistance Kurwanya cyane kugabanya ibihe nka hydrogène chloride, sulfurike, acetike na acide fosifori
Kurwanya aside hydrochloric kuri concentration zose n'ubushyuhe
● Mbere: INCONEL® alloy C-276 UNS N10276 / W.Nr.2.4819
Ibikurikira: HASTELLOY B-3 UNS N10675 / W.Nr.2.4600
Ikipe yacu ntabwo ari itsinda ryinzobere gusa zifite uburambe bwimyaka myinshi mubucuruzi mpuzamahanga.Turi abashya, duhora dushakisha imipaka y'ibishoboka.Gukoresha ibicuruzwa bigezweho nka Hastelloy B2 UNS N10665 W.NR.2.4617 byerekana ubushake bwacu bwo gukomeza imbere yaya marushanwa no gutanga serivisi nziza kubakiriya bacu.Twiyunge natwe mubushake bwacu bwo kugira ingaruka zirambye mu nganda kandi twiboneye imbaraga zo gutekereza guhanga udushya.