Nickel

Ibicuruzwa birambuye

Ibicuruzwa

Ubushyuhe bwo hejuru

◆ Nickel200 nubucuruzi bwera (99,6%) bukozwe muri nikel, bufite imiterere yubukanishi kandi irwanya ruswa nziza, amashanyarazi menshi n’umuriro w'amashanyarazi, gaze nkeya hamwe n’umuvuduko ukabije w’umwuka.

◆ Nickel201 (N02201) ni nikel yubucuruzi yuzuye ifite karubone nkeya cyane, byemewe gukorera ibidukikije kugeza 1230 ℃.

Ibigize imiti

Icyiciro

Ni

Fe

Cu

C

Mn

S

Si

Nickel200

99

≤0.4

≤0.25

≤0.15

≤0.35

≤0.01

≤0.35

Nickel201

99

≤0.4

≤0.25

≤0.02

≤0.35

≤0.01

≤0.35

Kugabanya umutungo ntarengwa

ifishi y'ibicuruzwa

imiterere

imbaraga zingana RmN / m㎡

Imbaraga Zitanga Rp0.2N / m㎡

Kurambura Nka%

Brinell gukomera HB

inkoni

ashyushye

60 ~ 85

15 ~ 45

35 ~ 55

45 ~ 80

inkoni

ubukonje bwashushanijwe cyangwa bufunze

55 ~ 75

15 ~ 30

40 ~ 55

45 ~ 70

isahani

annealing

55 ~ 80

15 ~ 40

40 ~ 60

45 ~ 75

flake

annealing

55 ~ 75

15 ~ 30

40 ~ 55

70 Hejuru

Umuyoboro w'icyuma

annealing

55 ~ 75

12 ~ 30

40 ~ 60

70 Hejuru