SUPER DUPLEX S32760 / F55 / 1.4501
GUSOBANURIRA
1.Gutanga imbaraga zisumba zombi austenitis na 22% Cr Duplex Stainless Steel UNS S32760 (F55) ikwiranye nuburyo butandukanye bukoreshwa mu nganda nka peteroli na gaze, CPI (Inganda zitunganya imiti), hamwe n’ibidukikije byo mu nyanja.
UNS S32760 (F55 / 1.4501) yanditse muri NACE MR 01 75 kubikorwa bya serivisi kandi imaze kubona ASME Icyemezo cya progaramu ya Vessel.
urwego rwimbaraga ukoresheje uburyo bworoshye bwo kuvura ubushyuhe kuri RH 950 na TH 1050. Imbaraga zidasanzwe zidasanzwe za Imiterere CH 900 zitanga ibyiza byinshi aho guhindagurika no gukora byemewe.Mu bushyuhe bwacyo butunganijwe, iyi mavuta itanga imiterere idasanzwe yubushyuhe bugera kuri 900 ° F (482 ° C).
Urupapuro rw'ibikoresho
Amavuta | Super Duplex S32760 |
Ibikoresho No. | 1.4501 |
Ikimenyetso cya EN (kigufi) | X2CrNiMoCuWN25-7-4 |
UNS | UNS S32760 |
Akarango k'akazi | ASTM A182 / F55 |
Ibigize imiti
C | Cr | Cu | Fe | Mo | Mn |
% | ≤% | ≤% | % | % | |
0.030 max | 24 <26 | 0.5 <1.0 | Kwibutsa | 3.0 <4.0 | 1.0 max |
N | Ni | P | S | Si | W |
% | % | % | % | ≤% | % |
0.20 <0.30 | 6.0 <8.0 | 0.030 max | 0.010 max | 0.010 max | 0.50 <1.0 |
Ibintu byihariye
Urubyiruko Modulus N / mm2 | Ubucucike kg / dm³: | Ubushobozi bwa Magnetique |
199 x 10³ | 7.81 g / cm³ | 33 |
Kurwanya Byiza Kurwanya no Gutobora / Isuri
Ibisobanuro
● EN 10088-3 1.4501
ASTM A473 UNS S32760 Kubabarirwa
● ASTM A182 Icyiciro F55 UNS S32760 Impimbano mpimbano
● ASTM A240 UNS S32760 Urupapuro nisahani
● ASTM A479 UNS S32760 Akabari
ASTM A276 UNS S32760 Imiterere A.
NACE MR 01-75
Ibikoresho bizana icyemezo cya 3.1.
3.2 ibyemezo birahari hamwe ninyongera.
Ibikoresho bya mashini
0.2% Ibimenyetso byerekana (N / mm2) [ksi] byibuze 550 | 550 [79.8] |
Imbaraga zidasanzwe (N / mm2) [ksi] byibuze | 750 [108.8]] |
Kurambura (%) byibuze | 25 |
Gukomera (HBN) | 270max |
Kugabanya igice cyambukiranya agace (%) byibuze | 45 |
Charpy V-notch Ingaruka kuri ibidukikije Temp (J) [ft.lb] | 80min [59min] |
Charpy V-Notch Ingaruka kuri -46 ° C (J) [ft.lb] | 45av, 35min [33av, 25.8min] |