Oy Alloy20cb-3 ifite imbaraga zo kurwanya ihungabana ryangirika no kurwanya kwangirika kwangirika kwangirika kwangirika, kandi ikoreshwa mubidukikije bya acide sulfurike no mu nganda zashizwemo na acide sulfurike irimo ion ya halogene na ion.
◆ Alloy28 ikoreshwa cyane mugukora impapuro, imiti, imiti, kurengera ibidukikije, kubaka ubwato nizindi nganda.
Oy Alloy31 (N08031 / 1.4562) ni azote irimo fer-nikel-molybdenum ivanze na azote ikora hagati ya super austenitis ibyuma bitagira umuyonga hamwe na nikel ishingiye kuri nikel.Irakwiriye kubya chimique na peteroli, inganda zidukikije n’ibicuruzwa bya peteroli na gaze, nibindi byinganda.
◆ Alloy33 ni ubwoko bwibyuma bikora igihe kirekire munsi yubushyuhe bwo hejuru bwa 600-1200 ℃ hamwe na stress zimwe.Ifite ubushyuhe bwo hejuru cyane, kurwanya anti-okiside no gukora ruswa.
◆ Alloy75 ifite umutekano mwiza kandi wizewe muri serivise mugihe cy'ubushyuhe bwinshi, kandi irakwiriye ikirere, indege, peteroli, inganda zikora imiti, nibikoresho byingenzi byubwato
Ibigize imiti
Icyiciro | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | Nb | ikindi |
ntarenze | ||||||||||||||
Inconel600 | 0.15 | 0.5 | 1 | 0.015 | 0.03 | 14 ~ 17 | shingiro | 6 ~ 10 | - | - | ≤0.5 | - | - | - |
Inconel601 | 0.1 | 0.5 | 1 | 0.015 | 0.03 | 21 ~ 25 | shingiro | 10 ~ 15 | 1 ~ 1.7 | - | ≤1 | - | - | - |
Inconel625 | 0.1 | 0.5 | 0.5 | 0.015 | 0.015 | 20 ~ 23 | shingiro | ≤5 | ≤0.4 | ≤0.4 | - | 8 ~ 10 | 3.15 ~ 4.15 | Co≤1 |
Inconel725 | 0.03 | 0.2 | 0.35 | 0.01 | 0.015 | 19 ~ 22.5 | 55 ~ 59 | Guma | 0.35 | 1 ~ 1.7 | - | 7 ~ 9.5 | 2.75 ~ 4 | - |
Inconel690 | 0.05 | 0.5 | 0.5 | 0.015 | 0.03 | 27 ~ 31 | ≥58 | 7 ~ 11 | - | - | ≤0.5 | - | - | - |
Kugabanya umutungo ntarengwa
Icyiciro | leta | imbaraga zingana RmN / m㎡ | Imbaraga Zitanga Rp0.2N / m㎡ | Kurambura Nka% | Brinell gukomera HB |
Amashanyarazi20cb-3 | Umuti | 600 | 320 | 35 | - |
Alloy28 | Umuti | 680 | 347 | 37 | - |
Alloy31 | Umuti | 650 | 350 | 35 | 25 |
Alloy33 | Umuti | 770 | 320 | 34 | - |
Alloy75 | Umuti | 750 | 310 | 37 | - |