◆ Inconel600 (N06600) ifite imbaraga zo kurwanya ruswa kubitangazamakuru bitandukanye byangirika, ifite kandi imbaraga nziza zo guturika, bisabwa kubikorwa bikora munsi ya 700 ℃.Ikoreshwa cyane mubijyanye no kubyaza umusaruro no gukoresha ibyuma byangiza alkali, cyane cyane mubidukikije aho sulfide ikoreshwa.
Performance Imikorere y'ingenzi ya Inconel601 (N06601) ni uko ifite imbaraga zo kurwanya okiside hamwe no kurwanya karuboni nziza mugihe ubushyuhe buri hejuru ya 1180 ° C. Ikoreshwa cyane cyane mubice bitunganya ubushyuhe, ibice bya sisitemu yo gusohora, hamwe nubushyuhe bwa ogisijeni.
◆ Inconel625 (N06625Ns336) yerekana imbaraga nyinshi zo kurwanya ruswa mu bitangazamakuru byinshi, kandi yoroheje yoroheje ya karuboni ntoya 625 ikoreshwa cyane mu nganda zitunganya imiti, aho ihuza amazi yo mu nyanja kandi ikihanganira imihangayiko ikomeye.
◆ Inconel725 ifite imbaraga zo kurwanya ruswa kandi irakwiriye kubikoresho byo mu miyoboro no mu nyanja.
◆ Inconel690 ifite anti-okiside na anti-ruswa, kandi irakwiriye kuri peteroli, metallurgie, ingufu za kirimbuzi, nibindi.
Ibigize imiti
Icyiciro | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | Nb | ikindi |
ntarenze | ||||||||||||||
Inconel600 | 0.15 | 0.5 | 1 | 0.015 | 0.03 | 14 ~ 17 | shingiro | 6 ~ 10 | - | - | ≤0.5 | - | - | - |
Inconel601 | 0.1 | 0.5 | 1 | 0.015 | 0.03 | 21 ~ 25 | shingiro | 10 ~ 15 | 1 ~ 1.7 | - | ≤1 | - | - | - |
Inconel625 | 0.1 | 0.5 | 0.5 | 0.015 | 0.015 | 20 ~ 23 | shingiro | ≤5 | ≤0.4 | ≤0.4 | - | 8 ~ 10 | 3.15 ~ 4.15 | Co≤1 |
Inconel725 | 0.03 | 0.2 | 0.35 | 0.01 | 0.015 | 19 ~ 22.5 | 55 ~ 59 | Guma | 0.35 | 1 ~ 1.7 | - | 7 ~ 9.5 | 2.75 ~ 4 | - |
Inconel690 | 0.05 | 0.5 | 0.5 | 0.015 | 0.03 | 27 ~ 31 | ≥58 | 7 ~ 11 | - | - | ≤0.5 | - | - | - |
Kugabanya umutungo ntarengwa
Icyiciro | leta | imbaraga zingana RmN / m㎡ | Imbaraga Zitanga Rp0.2N / m㎡ | Kurambura Nka% | Brinell gukomera HB |
Inconel600 | Umuti | 550 | 240 | - | ≤195 |
Umuti | 500 | 180 | - | ≤185 | |
Inconel601 | Annealing | 650 | 300 | - | - |
Umuti | 600 | 240 | - | 20220 | |
Inconel625 | Umuti | 760 | 345 | - | 20220 |
Inconel725 | Umuti | 790 | 485 | 28 | - |
Inconel690 | Umuti | 780 | 450 | 25 | - |